Why is TPV low hardness thermoplastic rubber agglomerated easily?
Text|Meite Polymer Tough Brother TPV particles As a general rule, we rarely see agglomeration of plastic particles, but thermoplastic elastomers are more prone to agglomeration, especially in low hardness specifications. The reas...
"Hermes" in floor mats - car mats made of thermoplastic elastomer TPE
Text|Meite milan polymer only An editor recently took advantage of Double Eleven and Double Twelve discounts to select car floor mats. Before buying, I studied knowledge of car mats on Internet: There are now dozens of floor mats ...
Table of plastic burning identification methods (worthy of a collection)
Plastic material\\ignition\\difficulty\\after going out of fire, whether it will change from \\flame state\\plastic change state\\smell Polyvinyl chloride (PVC)\\Difficult\\Extinguishing from fire\\yellow, green bottom, white smok...
Guessing root cause of TPE-S cracking (simple and clear, understanding is better than 10 years of experience)
Initial release | Durable polymer brother Meite 1. Definition of stress cracking: Stress cracking refers to phenomenon in which a polymeric material cracks and fails when subjected to prolonged stress below its yield strength or s...
Introduction to door and window sealing tapes and how to distinguish quality
Surface polymer finish Text\Meite Sealing tape is an inconspicuous detail in construction of doors, windows and curtain walls, but it plays a key role in use of doors and windows. Bottom sealing tapes for doors and windows cannot ...
The port cover of automotive high voltage line junction box is made of flame retardant TPV, and injection molding turns out to be defective when mixed with black masterbatch.
The port cover of automotive high voltage line junction box was originally used as TPV N1090AN in red and black, and main specifications are fine. TPV N1090AN is an off-white general purpose thermoplastic rubber. It is not flame...
Dual Cone Extruder Workflow - Speed, Temperature, Machine Switching (Actual Production)
Author: PVC Maniac The main control block of host's workflow is effect of host feed and speed on current, interaction between host temperature and recipe, and switching skills. 1. Adjust feeding speed according to speed of main ...
A brief description and a complete set of solutions on causes and measures to eliminate shrinkage marks in injection molding
Friendly reminder: Items 1-6 are relatively simple and clear. See summary of Part 7 at end of article for a detailed interpretation. 1. Definition Recess (Sink Mark) - when material cools and shrinks on a thick wall or in places ...
Introduction to water-swellable rubber
Water-swellable rubber (WSR) is a new type of specialty rubber that is made by physically mixing or chemically grafting hydrophilic components (or hydrophilic groups) and a rubber matrix under multiple expansion. It is known as a ...
Overview of Antistatics: Types and Mechanisms of Action of Antistatics
Original release | MET Polymer Zhong Ming 1. What is static electricity? When two solids with different physical states come into contact and rub against each other, their respective surfaces will redistribute charges. After re-se...